[USER=5796]@WARRIORWELDING[/USER]
So let me ask, why do I prefer wire speed 3-5/10 on hi on my cheap 90a hf fcaw unit regardless of thickness, when I crank it up to the recommended 9(say 3/16 1/4 plate), it doesn't make a puddle and just spatters and globs up? My guess is that it can't put enough power in to the wire to burn in. Maybe I'm just using the welder wrong or more likely it's just cheap crap.